Peeling, flaking, and Blistering paint

Causes

  • Because of the high humidity on the concrete wall, the paint blisters and peels off. This might be due to water leaking in various portions of the structure or a high moisture absorption from water uptake example Lower wall area.
  • The reason for this is because the surface before painting contains dirt, dust, and grease stains or inadequate surface cleaning, or has used the incorrect primer pain.
  • The paint coating has deteriorated with service life.

Solution

Step 1
Surface preparation

  1. Scrub and clean the old paint with water and a plastic brush.
  2. The surface must be completely clean and dry without any dust before painting.

Step 2
Primer

Nippon Paint Ultra Block Sealer

  1. Multi-purpose primer, suitable for high humidity area
  2. Solvent-based, excellent adhesion

Step 3
Topcoat

Nippon Paint Weatherbond

  1. Durable against harsh weather.
  2. Excellent UV reflection. Reduce substrate temperature to save energy costs.
  3. Excellent adhesion and durability for 15+ years.